Home / Halogen Line Heater / Halogen Line Heater Best Applications List / No.3 Dryness of paper-coating process

No.3 Dryness of paper-coating process

Dryness of paper-coating process  by the Halogen Line Heater

[ Problem Point ]

Had trouble without the location of the heater.

[ ⇒Kaizen Point ]

It was dry with 2M one Halogen Line Heater.

Strong light, enough output was able to be secured even in the small place.

Since the maximum temperature heated up in 5sec, immediately after the start of operation could work.The idling time vanished, the current spending 30 minutes in idling until PID steady.

In addition, the amount of electric use decreases, and the exhaust of CO2 has decreased, too.